@article{oai:kyutech.repo.nii.ac.jp:00004631, author = {Sun, Yong and 孫, 勇 and Kanemitsu, Shigeru and Kirimoto, Kenta}, issue = {2-1}, journal = {Pure and Applied Mathematic Journal}, month = {Dec}, note = {Dielectric properties of the Au/C60 (OH)24-26/Au structure were studied by measuring a.c. impedance and d.c. current in a wide temperature range. Three dielectric response characteristics were identified from Cole-Cole plots of a.c. impedance and dielectric dissipation factor of the structure. First, the bulk resistance and capacitance of the structure were observed at frequencies below 10 Hz, regardless of preparation condition of the Au electrode. Secondly, an interfacial characteristic of the Au foil/C60 (OH)24-26 contact was observed as a peak of dielectric dissipation factor at frequency of 200 Hz. Thirdly, an interfacial characteristic of the Au paste/C60 (OH)24-26 contact was also observed as a peak of dielectric dissipation factor at frequency of 1.7×〖10〗^5 Hz.}, pages = {18--24}, title = {Dielectric properties of Au/C60(OH)24-26/Au structure}, volume = {4}, year = {2014}, yomi = {ソン, ユー} }